Poor surface finish problems and solutions

发布时间:2020-11-26

went4.jpg

Poor surface finish problems and solutions


Problem 1. Feed speed is too fast or speed is too slow

Lower feed speed or increase RPM

Problem 2: Tool wear is serious

Change tool

Problem 3: The accuracy of the tool is not high after grinding

New tools are recommended for finishing

Problem 4: Too much chip accumulation

Remove cutting chips and change the cooling mode

Problem 5: Cutting fluid selection is not correct

Choose the right cutting fluid

Problem 6: Tool vibration is large

Select fixtures with high rigidity, high precision and strong grasp

  • Tool Products
    2020-12-08
    [2/3 edge] TA-Universal aluminum alloy milling cutter is suitable for general processing of aluminum alloy (Si≤12%) and copper alloy (<200HB) [2/3 edge] TA-universal aluminum alloy milling cutter is suitable for general processing of aluminum alloy (Si≤12%) and copper alloy (<200HB).
  • Industry Solution
    2020-12-08
    Tusa Precision Tools is a high-tech processing enterprise specializing in R&D, design, production and sales of carbide rotary tools for 3C electronics, mold, automotive, aerospace and aviation industries.
  • Tool  FAQ
    2020-12-08
    Tusa Precision Tools is a high-tech processing enterprise specializing in R&D, design, production and sales of carbide rotary tools for 3C electronics, mold, automotive, aerospace and aviation industries.
  • Sample & Guide
    2020-12-08
    Tusa Precision Tools is a high-tech processing enterprise specializing in R&D, design, production and sales of carbide rotary tools for 3C electronics, mold, automotive, aerospace and aviation industries.

服务热线

139 2550 6324

微信号

刀具定制询价

* * * * * *上传附件,图纸 *刀具类型、工件材料、刃径、刃长、刃数、柄径、总长、是否涂层、是否高光、订购数量、其他特殊要求